10815L
Chemical
- Jul 24, 2011
- 178
Hi,
I'm commissioning a gas plant and for heat medium using therminol 66 by eastman company. the problem is being faced is that mahle wound type filter element elements were found decomposed even temperature was only 125^0c.
Thus anyone can explain why filter elements are decomposed even delta pressure against filter was only 30 psig.
Thanks
10815L
I'm commissioning a gas plant and for heat medium using therminol 66 by eastman company. the problem is being faced is that mahle wound type filter element elements were found decomposed even temperature was only 125^0c.
Thus anyone can explain why filter elements are decomposed even delta pressure against filter was only 30 psig.
Thanks
10815L