Minimum applicable working temperature

Status
Not open for further replies.

farzam

Mechanical
Nov 4, 2002
79
Dear All,

please let me know, the mimum applicable working temperature for P-265GH and P-245GH.is it possible to use them for -20C temperature? (thk.<16mm)

Thanks in advance
 
Replies continue below

Recommended for you

farzam;
The Carbon Steel Handbook by EPRI is now available on the public domain. Locate a copy and you will find that the above pressure vessel steel grades under CEN standards are comparable to the following ASTM/ASME specifications;

CEN 10222-2 P245GH is comparable to ASTM/ASME A/SA 350 LF1
CEN 10222-2 P265GH is comparable to ASTM/ASME A/SA 516 Gr 60

Yes, both steels supplied to the above CEN standards can be used at -20 deg C.

 