I have a moment frame for a screened porch that is not working very hard. It is resisting mainly wind loads. It is a W10x22 beam on top of an HSS5x5. Based on the numbers, fillet welds will work. Any reason I would have to use full-penetration welds?
 
Replies continue below

Recommended for you

Then why provide the HDG option on the TBs?
Who knows? Regardless, the coating will not survive the self tapping process.
 
Last edited:
I design those as enclosed / open structure as I've never found anything on wind loads through screens.

I was more getting at the moisture effects on connection strength, as those cam get pretty onerous.
 