HDS
Mechanical
- Jul 25, 2002
- 661
What are the options for making a small tank? I want to make sure I have considered all the options for this design.
Here are the details:
500ml
2psi internal pressure
needs to be water tight
contents will be liquid cleaners (originally sold in PD jugs)
5000 parts a year
The processes I know of are:
rotomolding
blow molding
injection molding as two halves and welding together
What other options are there? Even something obscure or unusual would be fine.
TIA
Here are the details:
500ml
2psi internal pressure
needs to be water tight
contents will be liquid cleaners (originally sold in PD jugs)
5000 parts a year
The processes I know of are:
rotomolding
blow molding
injection molding as two halves and welding together
What other options are there? Even something obscure or unusual would be fine.