QCJT
Industrial
- Feb 16, 2011
- 52
Our client doubts if we have achieved a necessary level of insulation inside a header, so we need to measure it's thickness somehow. Thickness measurement of two layers of dried refractory without destroying its integrity seems impossible. So we decided to try to use rebar detectors to measure cover of the stainless steel anchors inside the cast refractory. If that is of proper thickness then same applies to the rest. I'm not sure however if the rebar detectors (such as Profometer's scanlog) are able to work on 95% alumina content refractory.
Besides an opinion about the above I'd appreciate recommendations on how to measure thickness of the refractory in the header.
Besides an opinion about the above I'd appreciate recommendations on how to measure thickness of the refractory in the header.