JohnRwals
Structural
- Jul 8, 2020
- 151
Was AWS D1.4 revised recently about the filler metal requirement?
PCI Design Handbook used to say E70 and E80 could be used.
Now it shows only E80 can be used for A706 Gr. 60 rebar welding.
Can I use E70 with longer welding instead of E80?
I would like to know why PCI changed these welding tables.
Thanks!
John
PCI Design Handbook used to say E70 and E80 could be used.
Now it shows only E80 can be used for A706 Gr. 60 rebar welding.
Can I use E70 with longer welding instead of E80?
I would like to know why PCI changed these welding tables.
Thanks!
John