I am intending to manufacture a Pressure Vessel Housing (cylindrical shaped over 4" Bore). I note that SA-564 type 630 H1150 requires a minimum reduction in area of 50% for material sizes up to 8". The material I intend to use is greater than 8" therefore am I correct in assuming when I conduct the additional transverse tests in accordance with code case 2156-1, then the minimum required reduction of area is 30%?