Hello
I have storage tank made from SA516 gr 60 material. Tank covered by API 650. Please look at my inerpretation of impact testing energy value. It is important for me.

API 650 twelfth ed. 2013
SA516-60 in table 4.4b -> material group III or IIIA
Table 4.5a -> min value 20J

Thanks in advance for any help
 
Replies continue below

Recommended for you

What is the minimum impact test temperature for 20J?
 
If the SA 516 Gr 60 plate was supplied in a normalized condition, I don't see a problem.
 
What exactly is the question: is it 'am I reading the standard correctly?'

The minimum individual requirement for one longitudinal test piece of the three only is 13 J. 20 J is the minimum average value where at least two of the three longitudinal test pieces achieve this value.

Not at all onerous for a reasonably average heat of normalised A516.



Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
Thanks all for answers
I am not an expert in API650 therefore this question
Regards
 