In twenty years I've never been asked nor have i considered this:
The General Contractor wants to know where to put their typical 1/4" wide x 1" control joint cuts in the precast concrete topping.
The typical standard with this G.C. is 156 SF max concrete area for saw-cut boundaries.
The current project is 10" hollowcore precast plank with 4" structural, 4,000 psi concrete topping.
Approximate camber = 1".
Our plan specifies 6"x6" #10/10 W.W.M.
Do any of you ever specify saw-cuts in structural precast concrete topping?
I will also be contacting the precast supplier for advice and guidance.
Thank you!
The General Contractor wants to know where to put their typical 1/4" wide x 1" control joint cuts in the precast concrete topping.
The typical standard with this G.C. is 156 SF max concrete area for saw-cut boundaries.
The current project is 10" hollowcore precast plank with 4" structural, 4,000 psi concrete topping.
Approximate camber = 1".
Our plan specifies 6"x6" #10/10 W.W.M.
Do any of you ever specify saw-cuts in structural precast concrete topping?
I will also be contacting the precast supplier for advice and guidance.
Thank you!