Lahane
Mechanical
- Jul 23, 2010
- 27
I already have a PQR (P1G1 TO P1G2) qualified with EH10K filler wire & F7A6/P6 EH10K Flux by SAW process with PWHT.
Now the customer spec say high manganese fillers are not to be used to weld the Carbon steel material.
Which filler & Flux I should go for?Does I have to qualify a new PQR with changed filler.What i will need to do to avoid a new PQR qualification?
Thanks in advance.
Now the customer spec say high manganese fillers are not to be used to weld the Carbon steel material.
Which filler & Flux I should go for?Does I have to qualify a new PQR with changed filler.What i will need to do to avoid a new PQR qualification?
Thanks in advance.