I'm doing an analysis for an aluminum dock. The legs are square tubing inside square tubing. A 1/2 inch by 13 bolt is threaded through the outside tubing and pushes up against the inside tubing. In a set bolt kind of fashion. I need to calculate how much force can be applied to the inside (moveable) square tubing before it slips. I'm looking for a way to calculate how much torque applied to apply to the bolt.and the resorting force on the inside tubing. any ideas?