Hi, I hope someone can help me.
I have designed some specific application machinery and one of the processes is a twin screw extruder for making powder coatings, I designed this machine two years ago, made it and have been using the machine now for over a year. originally it was only meant to be a prototype just to see if it worked, ie did it make powder coatings, anyway it did and I have developed a business around this extruder.
The problem is now the gearbox, the shafts last about 2 months and then fail. I recently redesigned the mechanics basically beefing up the shafts diameters etc. My question is: Previously (whilst living in England) I always used En24T, turned the shaft, installed and ran and I always had good luck with it. Here in the States I have had trouble with steels, Does anyone know a decent equivelent to En24T (is it 4340 - chemically similar but is it equiv in physical properties?) I also used 1144 on advise from our steel stockist, but I think he had another motive. OR - does anyone know where I can get En24T from in USA?
I have designed some specific application machinery and one of the processes is a twin screw extruder for making powder coatings, I designed this machine two years ago, made it and have been using the machine now for over a year. originally it was only meant to be a prototype just to see if it worked, ie did it make powder coatings, anyway it did and I have developed a business around this extruder.
The problem is now the gearbox, the shafts last about 2 months and then fail. I recently redesigned the mechanics basically beefing up the shafts diameters etc. My question is: Previously (whilst living in England) I always used En24T, turned the shaft, installed and ran and I always had good luck with it. Here in the States I have had trouble with steels, Does anyone know a decent equivelent to En24T (is it 4340 - chemically similar but is it equiv in physical properties?) I also used 1144 on advise from our steel stockist, but I think he had another motive. OR - does anyone know where I can get En24T from in USA?