i have shifted to a new home and wondering which piping connection will suits best for my requirement. I have been using black pipe nipples from shanghai rolling threads since past 2 years and it worked perfectly fine for me. It just need to ask that either black pipes works exactly the same for water piping or should i choose some other option.
 
Replies continue below

Recommended for you

Black steel pipe is acceptable for gas pipe, but I would not use it for water pipe, nor is it allowed in the International Plumbing Code.
 
Black pipe would start leaking from corrosion within a few years of water service.
 
Black only for Gas
Galvanized only for Water

Using Galvanized on gas can result in zinc debris ending up clogging a valve or nozzle in your gas appliance.
 
Use copper for potable water. It is anti-microbial and is a proven winner.

As a side note, I grew up in a house with galvanized and black steel pipe for water and gas. No problems that I remember.
 
Galvanized pipe will work but it will have a limited lifetime as galvanized pipe is susceptible to corrosion and scaling.

The plumbing industry seems to moving to PEX.
 
Correcting my post above to make it more explanatory:

Galvanized pipe will work for water service but galvanized pipe will have a limited lifetime as galvanized pipe is susceptible to corrosion and scaling when used for water service.

The plumbing industry seems to moving to PEX for water service.

[URL unfurl="true" said:
https://www.uponor-usa.com/residential-plumbing.aspx[/URL]]PEX

You may use GasFlex for gas service:

[URL unfurl="true" said:
http://www.gasflex.com/[/URL]]GasFlex

Some areas allow galvanized pipe for gas service as well.

Tip: Always check local code requirements to confirm that the materials you select meet required standards.
 