Hi heat exchanger design experts,
Does the tube expansion depth ration apply for the light expanded (closing the gap between tube and tube hole) of the tube to tube sheet joint? I think it should not, it should not consider the tube expansion depth ratio 'ρ' for the Effective Ligament Efficiency = (p✱ - d✱)/p✱, but code dose not clear mention it. ρ = tube expansion depth ratio = ℓ t x /h ,(0 ≤ ρ ≤ 1).
My understanding is,
Strength weld+light expanded(thickness reduction<2%)= Strength weld is joint type "a" in ASME VIII-1, Table A-2, Efficiencies fr.
Strength weld+heavy expanded is joint type "e" in ASME VIII-1, Table A-2, Efficiencies fr.
Regards,
Does the tube expansion depth ration apply for the light expanded (closing the gap between tube and tube hole) of the tube to tube sheet joint? I think it should not, it should not consider the tube expansion depth ratio 'ρ' for the Effective Ligament Efficiency = (p✱ - d✱)/p✱, but code dose not clear mention it. ρ = tube expansion depth ratio = ℓ t x /h ,(0 ≤ ρ ≤ 1).
My understanding is,
Strength weld+light expanded(thickness reduction<2%)= Strength weld is joint type "a" in ASME VIII-1, Table A-2, Efficiencies fr.
Strength weld+heavy expanded is joint type "e" in ASME VIII-1, Table A-2, Efficiencies fr.