i've just poured a waffle roof slab(flat) of a single family home. The beams are 6"x6" spaced 24" in both directions with 4-#3rebars and its slab is 3".
Now here comes my problem. The structural engineer specified the concrete resistance at 200kg/cm2 and they used 150kg/cm2. The structural engineer is not in town so I came here....
How critical is it?
*Attached is a JPEG
The area in red is my concern since it spans +/-14'
Everything is in centimeters.