Hi everyone,
I would like to start a discussion on the use of anti seize on vehicle lug nuts. Searching the net, there are people that claim to have used anti seize on lug nuts for many years with no problems, and some people that advise against it.
I have two main questions I would like to address separately. The two questions directly below are related to the two main sources of controversy on the subject.
1. Will the use of anti seize on properly torqued vehicle lug nuts likely cause them to loosen over time, to the point where it could be dangerous ?
2. Will the use of anti seize on vehicle lug nuts cause a significant increase in the axial loads and/or stresses on the lug studs, that would likely cause a significant problem or danger ? If so, I would think you could simply reduce the specified torque by a certain percentage to compensate for the use of the anti seize.
I have a bottle of NAPA anti seize (item # 765-1674) and interestingly enough, it says right on the bottle to use anti seize on lug nuts.
I would expect most engineers and auto manufacturers to recommend not to use anti seize on lug nuts, even if they're not sure either way whether or not it would cause any problems, just because of safety liability.
On the other hand, one would think that a large company like NAPA also considered safety liability, and would not state right on the product bottle to use anti seize on lug nuts, unless it was a safe practice.
On the bottle of the NAPA anti seize product mentioned above, under directions, it states to apply the product, and then torque all bolts to manufacturers specifications.
The directions make no torque reduction allowance for the lubrication effects of the anti seize, and the effects it may have on increasing axial loads beyond those anticipated at OEM specified torques.
Also on the NAPA anti seize bottle, it recommends the use of the product on engine head bolts, but again, does not provide any recommendation for an OEM torque spec reduction with the use of the anti seize, which leads one to believe that it may not be a significant issue.
Most repair shops are not going to torque your wheels anyway, they will use impact wrenches which always over torque and many times warp rotors. Some shops use torque sticks on the end of the impact wrenches which is a good idea, but you would be hard pressed to find any shop using torque wrenches on lug nuts. It's just not fast enough for them. Even if you request that they use a torque wrench, they may likely forget, so you would have to watch them. I know because years ago I worked in an auto repair shop.
I have used anti seize on the lug nuts of one vehicle I have and I have not had any problems. I used it very sparingly, and I tried my best to make sure that there was no anti seize between the end of the lug nut (part that seats in the rim) and the rim. These were aluminum rims with closed end acorn style lug nuts. I re torqued after driving 50 miles or so which is standard practice on aluminum rims anyway.
The reason I used the anti seize is because I had to remove a tire once and the lugs were so rusted I could not remove the nuts without a breaker bar. I thought they might break. After that, I removed the lugs on all the wheels, replaced them with new lug nuts, and applied a small amount of anti seize to each lug stud at the time of replacement. That was years ago and I have not had any problems.
Many times cars will come into a repair shop with rusted lugs. Some lugs will come off with an impact wrench and others will break off because they are too rusted. However, just because the lug nut came off with an impact does not mean that the stud was not damaged, fractured, or over stressed when removing the lug nut, due to the corrosion present. This is another reason I can think of to apply something to lug nuts and studs to keep them from rusting.
Is there anyone out there that has had some real world experience with this, perhaps with fleet vehicles ?
I would appreciate any feedback or thoughts.
Thanks
John
I would like to start a discussion on the use of anti seize on vehicle lug nuts. Searching the net, there are people that claim to have used anti seize on lug nuts for many years with no problems, and some people that advise against it.
I have two main questions I would like to address separately. The two questions directly below are related to the two main sources of controversy on the subject.
1. Will the use of anti seize on properly torqued vehicle lug nuts likely cause them to loosen over time, to the point where it could be dangerous ?
2. Will the use of anti seize on vehicle lug nuts cause a significant increase in the axial loads and/or stresses on the lug studs, that would likely cause a significant problem or danger ? If so, I would think you could simply reduce the specified torque by a certain percentage to compensate for the use of the anti seize.
I have a bottle of NAPA anti seize (item # 765-1674) and interestingly enough, it says right on the bottle to use anti seize on lug nuts.
I would expect most engineers and auto manufacturers to recommend not to use anti seize on lug nuts, even if they're not sure either way whether or not it would cause any problems, just because of safety liability.
On the other hand, one would think that a large company like NAPA also considered safety liability, and would not state right on the product bottle to use anti seize on lug nuts, unless it was a safe practice.
On the bottle of the NAPA anti seize product mentioned above, under directions, it states to apply the product, and then torque all bolts to manufacturers specifications.
The directions make no torque reduction allowance for the lubrication effects of the anti seize, and the effects it may have on increasing axial loads beyond those anticipated at OEM specified torques.
Also on the NAPA anti seize bottle, it recommends the use of the product on engine head bolts, but again, does not provide any recommendation for an OEM torque spec reduction with the use of the anti seize, which leads one to believe that it may not be a significant issue.
Most repair shops are not going to torque your wheels anyway, they will use impact wrenches which always over torque and many times warp rotors. Some shops use torque sticks on the end of the impact wrenches which is a good idea, but you would be hard pressed to find any shop using torque wrenches on lug nuts. It's just not fast enough for them. Even if you request that they use a torque wrench, they may likely forget, so you would have to watch them. I know because years ago I worked in an auto repair shop.
I have used anti seize on the lug nuts of one vehicle I have and I have not had any problems. I used it very sparingly, and I tried my best to make sure that there was no anti seize between the end of the lug nut (part that seats in the rim) and the rim. These were aluminum rims with closed end acorn style lug nuts. I re torqued after driving 50 miles or so which is standard practice on aluminum rims anyway.
The reason I used the anti seize is because I had to remove a tire once and the lugs were so rusted I could not remove the nuts without a breaker bar. I thought they might break. After that, I removed the lugs on all the wheels, replaced them with new lug nuts, and applied a small amount of anti seize to each lug stud at the time of replacement. That was years ago and I have not had any problems.
Many times cars will come into a repair shop with rusted lugs. Some lugs will come off with an impact wrench and others will break off because they are too rusted. However, just because the lug nut came off with an impact does not mean that the stud was not damaged, fractured, or over stressed when removing the lug nut, due to the corrosion present. This is another reason I can think of to apply something to lug nuts and studs to keep them from rusting.
Is there anyone out there that has had some real world experience with this, perhaps with fleet vehicles ?
I would appreciate any feedback or thoughts.
Thanks
John