There is a ball that is used for form metal in a spinning process which includes hot spinning. Ideal material would have high abrasion resistance, high toughness and suitable for high temperature use (surface temperatures up to ~1300F).
Ball size: 40” OD (39.370” finished OD) x 11.5” ID (11.811” finished ID) x 25” Long (23.622” finished length) Casting, Approximate Weight 7,400 lbs
I've ruled out any castings with significant amounts of chrome (over 0.5%) because it increases brittleness; all ASTM A532 materials.
Any suggestions on material grades that should be considered?
Thank you for your time
A Fan of EngTips, share the knowledge
There is a ball that is used for form metal in a spinning process which includes hot spinning. Ideal material would have high abrasion resistance, high toughness and suitable for high temperature use (surface temperatures up to ~1300F).
Ball size: 40” OD (39.370” finished OD) x 11.5” ID (11.811” finished ID) x 25” Long (23.622” finished length) Casting, Approximate Weight 7,400 lbs
I've ruled out any castings with significant amounts of chrome (over 0.5%) because it increases brittleness; all ASTM A532 materials.
Any suggestions on material grades that should be considered?
Thank you for your time