DogPAnt
Electrical
- Apr 20, 2023
- 3
I hope I'm in the appropriate forum.
I'm potting some electronics in epoxy (BEEP 6112).
I'm having water ingress problems and suspect it is due to a weak bond to the PVC sheathed wires going into the potted part.
I think water is leaking in along the interface between the PVC sheath and the epoxy.
The water works its way in over a few days.
Is there a simple way to improve this bond?
I've been trying to find a readily available compound to work as an intermediary that bonds well to epoxy AND PVC. Hopefully something that I can simply paint onto the wire sheath.
I'm only looking at up to say 10m depths.
Any ideas?
Thanks
I'm potting some electronics in epoxy (BEEP 6112).
I'm having water ingress problems and suspect it is due to a weak bond to the PVC sheathed wires going into the potted part.
I think water is leaking in along the interface between the PVC sheath and the epoxy.
The water works its way in over a few days.
Is there a simple way to improve this bond?
I've been trying to find a readily available compound to work as an intermediary that bonds well to epoxy AND PVC. Hopefully something that I can simply paint onto the wire sheath.
I'm only looking at up to say 10m depths.
Any ideas?