Hi all,
Do we need to include weld-leg size in calculating 'c1' & 'c2' values (rectangular attachment)?
If I have a rectangular attachment of L=5" and W=3" with a weld-leg size of 0.25". Which one is correct below?

Method-A:
c1 = 3/2 = 1.5"
c2 = 5/2 = 2.5"

Method-B:
c1 = 3/2 + 0.25 = 1.75"
c2 = 5/2 + 0.25 = 2.75"

Similarly, what will be the case in the circular attachment? Does 'Ro' value include weld-leg size?

I have found Codeware-Compress including weld-leg size for rectangular attachment and not using in circular attachment.

I really appreciate any help you can provide.
Thanks
 
Replies continue below

Recommended for you

Don't worry that much. Use method B and round attachment without considering weld size to ease your life. For sure you can add weld to round attachment, but no one cares about it.
 
If the load assumptions used in the derivation were uniform load over a round or rectangular area, I'd just use the plate size.
If they assumed line loads in a square or circle shape, I'd figure center of throat of weld.
In either case, the design is rather approximate, so there may not be a practical difference.
 