Sep 22, 2004 #2 SAE79 Chemical Sep 22, 2004 2 US Al(OH)3 alumina trihydrate has a heat capacity of approximately 0.24 BTU/lb*deg F. AlF3 (aluminium trifluoride)should have a comparable value. I am not familiar with aluminum trifluoride trihydrate. Upvote 0 Downvote
Al(OH)3 alumina trihydrate has a heat capacity of approximately 0.24 BTU/lb*deg F. AlF3 (aluminium trifluoride)should have a comparable value. I am not familiar with aluminum trifluoride trihydrate.
Sep 23, 2004 Thread starter #3 djoko Chemical Jan 3, 2003 10 ID sae79... i mean AlF3.3H2O aluminum fluoride trihydrate. sorry for the wrong name and thank you for your info. djoko Upvote 0 Downvote
sae79... i mean AlF3.3H2O aluminum fluoride trihydrate. sorry for the wrong name and thank you for your info. djoko