I saw a show the other day about the inventor of the compressed air powered car. The show stated he worked for a forumla one team for a number of years as an internal engine components engineer. They said he was know for first using magnesium in piston contruction to get piston weight in these engines down to around 250 grams. Wow! Does anyone know if this was an alloy and if so what might be the ratio of magnesuim to aluminum?