spyros_ar
Student
- Jun 1, 2021
- 10
Dear all,
I am performing a linear buckling analysis of a sandwich structure, specifically a tapered cylindrical shell with reinforced patches. The face sheets are modeled using conventional S4R shell elements and are tied to the core vie TIE constraints. For the core, I used two different approaches:
I am performing a linear buckling analysis of a sandwich structure, specifically a tapered cylindrical shell with reinforced patches. The face sheets are modeled using conventional S4R shell elements and are tied to the core vie TIE constraints. For the core, I used two different approaches:
- Solid C3D8I elements (4 elements across the thickness).
- Continuum shell elements.