from the CBC, "In the wake of a fatal transmission line tower collapse in Newfoundland and Labrador, the Manitoba Federation of Labour is calling on Manitoba Hydro to make sure workers doing similar work in this province are safe.
"I hope these things are being looked at seriously and I'm very fearful," said MFL president Kevin Rebeck, worried that the accident in Newfoundland could be repeated in Manitoba. 5 Manitoba Hydro transmission towers collapse during assembly.
Condolences pour in as Forbes Bros. confirms 2 employees killed in transmission tower collapse. Two workers died Monday when a steel transmission tower collapsed while being built near Come by Chance, N.L.
Manitoba Hydro has had five transmission towers collapse between February and May this year, although there were no injuries reported in the Manitoba incidents."
There have been large staff cut-backs at Manitoba Hydro of late.
Dik
"I hope these things are being looked at seriously and I'm very fearful," said MFL president Kevin Rebeck, worried that the accident in Newfoundland could be repeated in Manitoba. 5 Manitoba Hydro transmission towers collapse during assembly.
Condolences pour in as Forbes Bros. confirms 2 employees killed in transmission tower collapse. Two workers died Monday when a steel transmission tower collapsed while being built near Come by Chance, N.L.
Manitoba Hydro has had five transmission towers collapse between February and May this year, although there were no injuries reported in the Manitoba incidents."
There have been large staff cut-backs at Manitoba Hydro of late.
Dik