bugbus
Structural
- Aug 14, 2018
- 533
Follow along with the video below to see how to install our site as a web app on your home screen.
Note: This feature may not be available in some browsers.
In a city council meeting, the City of Hickory says they will not be conducting an independent investigation into the collapse of two arches over the City Walk pedestrian bridge over Highway 27 on Feb. 18.
Officials say the city never accepted ownership of the arches. Officials say the project was technically incomplete until the DOT signs off and the city formally takes ownership.
....
The North Carolina Department of Transportation owns the bridge, according to Hickory City Council. Therefore, the city does not have the authority to remove the arches, so other parties will have to remove them.
....
The city says multiple groups are investigating and developing reports on why this happened. The city is not one of those groups investigating. Officials say the insurance company advised the city not to get involved in the investigation.