RetiredSE
Structural
- Mar 22, 2018
- 5
There appears to be a cold joint in 11-12 at the top of the deck. See photos above. If the PT rod(s) is anchored below that point, somewhere lower in the deck, and you increase the PT force, you increase the shear along the cold joint.